潜在失效模式及后果分析(FMEA)常用语
发布人:圣才学习网  发布日期:2010-08-25 10:20  共人浏览[] [] []
  设计/过程FMEA design/process FMEA
  项目名称(item
  主要参加人员(core team
  设计/过程责任部门(design/process responsibility
  关键日期(key date
  编制(prepared by
  审批(approved by
  过程功能(process function
  要求(requirements
  潜在失效模式(potential failure mode
  潜在失效后果(potential effects of failure
  严重度数(severity 级别(classification
  潜在的失效起因/机理(potential causes/mechanisms of failure
  频度数(occurrence
  现行过程控制(current process control
  预防(prevention
  探测(detection
  风险顺序数(risk priority number
  建议的措施(recommended actions
  责任和目标完成日期(responsibility & target completion date
  措施结果(action results
  采取措施(actions taken ?
  影响产品特性/二次加工周期/外观/装配功能(affect product characteristic/ postprocessing period/ appearance/assembling function
  用料不符合要求(inconformable material to the requirements
  温度控制不当(incorrect temperature control
  模具/机板不平行(die/machine platen in unparallel
  锁模力过小(lack of locking force
  模具温度过低(lower die temperature
  射料力/打锤时间不足(lack of injection force/shot time
  料温过低/过高(lower/excessive metal temperature
  模具过热(excessive hot die
  运水量过低(lower volume of cool water
  喷雾过大(release agent to excess
design翻译  射速太快(rapid injection velocity
  喷雾频次过少或喷雾不均匀(infrequent/ uneven spraying release agent
  模温过高导致蚀模(excessive hot die leads to die corrosion
  模具尺寸不符合要求(die size out of the specification
  工模行位柯磨损(core slides worn out
  开模时间过短(shortage of dieopen time
  顶出时间过短(shortage of ejector time
  冲剪夹具有缝隙(trimming die with crack
  操作时摆放不正确(lay products in disorder during operation
  除批锋时操作不当而刮伤表面(surface scratch due to the improper handling in removing flash
  摆放不正确堆积产品(pile products up due to laying in disorder
  磨光轮选择不合适(unsuitable polishing wheels
  布轮(polishing/cotton wheels
  麻轮(sisal/sisal buffing wheels
  砂布轮(sanding wheels
  铜丝轮(brass brush wheels
  磨料(abrasive medium ?
  手工磨光(manual polishing
  抽取样品时产品有碰撞(bump at sampling
  货与货之间碰撞(bump among products
  电子磅误差超标(digital balance out of allowable error
  主管对员工培训不足(lack of necessary training for employees
  按工作指示设定压铸参数/锁模力/射料力/射料速度/打锤时间/喷雾量/开模时间/顶出时间/压力参数/料温/控制温度/作业(set diecasting parameter/locking force/ injection force/injection velocity/shot time/ volume of release agent/dieopen time/ ejector time/pressure rating/metal temperature/ control temperature/ operation according to WI
  开拉前培训(training before operation
  定期校准电子磅(regular calibration for digital balance

版权声明:本站内容均来自互联网,仅供演示用,请勿用于商业和其他非法用途。如果侵犯了您的权益请与我们联系QQ:729038198,我们将在24小时内删除。